Amerchol (A subsidiary of The Dow Chemical Company)
| A. | |
| Water (aqua) | qs |
| B. | |
| Polyquaternium-67 (SoftCAT SX-400X Polymer (1% aq.), Dow Chemical) | 20.00%w/w |
| C. | |
| Water (aqua) | qs |
| D. | |
| Carbomer, 3% aq. (Carbopol 980, Noveon) | 13.55 |
| E. | |
| Water (aqua) | 23.80 |
| F. | |
| Cocoamidopropyl betaine (35% solids) | 5.70 |
| G. | |
| Sodium laureth sulfate (2 moles - 70% solids) | 20.00 |
| Tetrasodium EDTA | 0.10 |
| H. | |
| Triethanolamine | qs |
| I. | |
| Glycol distearate (and) laureth-4 (and) cocamidopropyl betaine (Euperlan PK 3000 AM, Cognis) | 4.65 |
| J. | |
| DMDM hydantoin | 0.40 |
| K. | |
| INCI Not Provided (Dow Corning 2-1310BB Emulsion, 3.30) | qs |
| Sodium chloride | 0.50 |
| Fragrance (parfum) | qs |
| L. | |
| Decyl glucoside (50% solids) | 8.00 |
Procedure: Sprinkle B into A at RT with agitation. Allow to disperse completely before beginning to heat slowly. With mixing, heat to 60-65°C. Let cool to RT. Solution should be clear. Set aside. Sprinkle D into C at RT with agitation. Continue mixing until completely dispersed. Do not neutralize. Set aside. In main vessel, combine AB and E. Mix with heating to 70-75°C. Add F. Once uniform, add CD. Continue mixing. In separate vessel, combine G. Heat to 70-75°C, mixing until disolved. Add G to batch with mixing. Adjust pH to 6.0-6.5 with H. Cool to 35-40°C while mixing. Add I and mix until uniform. Add J. Cool to RT. Add K to batch and mix until completely uniform. Adjust to pH 6.0-6.5 using L.