Colonial Chemical Inc.
| A. | |
| Water (aqua) | 51.65%w/w |
| B. | |
| Carbomer 940 | 0.25 |
| C. | |
| Triethanolamine, 99% | 0.40 |
| D. | |
| Water (aqua) | 30.00 |
| Stearamidopropyl PG-dimonium chloride phosphate (Cola Lipid ST, Colonial Chemical) | 1.00 |
| E. | |
| SD3A alcohol | 15.00 |
| F. | |
| Phenyl dimethicone | 1.50 |
| Titanium dioxide | 0.20 |
| G. | |
| Preservative | qs |
| Fragrance (parfum) | qs |
| Color | qs |
Procedure: Slowly add B to A with good agitation until dissolved. Add C. In a separate container, mix D and heat to 65 1/2°C with mixing. When dissolved, cool to 30-35 1/2°C and add E. Add DE to ABC, mixing well. Add F to the slurry. Blend together until a uniform white lotion is obtained. Add G.