New Phase Technologies
| A. | |
| C20-40 Alcohols (Performacol 425 Alcohol, New Phase Technologies) | 4.00%w/w |
| Polyethylene (Performalene 400 Polyethylene, New Phase Technologies) | 1.00 |
| Cyclopentasiloxane (SF1202, General Electric) | 60.00 |
| Dimethicone (SF96-100, General Electric) | 10.00 |
| B. | |
| Aluminum zirconium tetrachlorohydrex GLY (Reach AZP-908, Reheis) | 25.00 |
Procedure: Heat A to 92-95ºC. Mix until dispersed and uniform while keeping covered. Add B to A with high shear mixing. After fully dispersed, remove from heat.