Dow Corning Corp.
| A. | |
| Water (aqua) | 58.45%w/w |
| Glycerin | 5.00 |
| PVP/VA copolymer (Luviskol VA-64E, BASF) | 10.00 |
| B. | |
| Sodium polyacrylate (and) dimethicone (and) cyclopentasiloxane (and) trideceth-6 (and)PEG/PPG-18/18 dimethicone (Dow Corning RM 2051 Thickening Agent, Dow Corning) | 4.00 |
| C. | |
| Beeswax | 3.00 |
| Petrolatum | 5.00 |
| Cetyl alcohol | 3.00 |
| C30-45 alkyl methicone (and) C30-45 olefin (Dow Corning AMS-C30 Cosmetic Wax, Dow Corning) | 2.00 |
| Dimethicone (Dow Corning 225 Fluid, Dow Corning) | 2.00 |
| Phenyl trimethicone (Dow Corning 556 Fluid, Dow Corning) | 2.00 |
| Mangifera indica (mango) seed butter (Dow Corning HY-4001 Mango Butter, Dow Corning) | 3.00 |
| Caprylic/capric triglyceride (Myritol 318, Henkel KGaA) | 2.00 |
| D. | |
| Propylene glycol (and) diazolidinyl urea (and) iodopropynyl butylcarbamate (Liquid 0.45 Germall Plus, ISP Sutton Laboratories) | 0.45 |
| Fragrance (parfum) | 0.10 |
Procedure: Combine A with mixing. Heat to 80°C. Add B to A. The mixture will quickly become very viscous. Mix with agitation to obtain a homogeneous mixture. In a separate vessel, combine C and heat to 80°C with gentle mixing until all wax is melted and mixture is uniform. Add C to AB over about 3 min, while stirring at less than 1500 rpm. Reduce mixer speed to 500 rpm and continue stirring as the batch cools to RT. Add D and mix until homogeneous.