Formula 3. Protective lotion

A.
Water (aqua), qs to 100.00% w/w

B.
Beta Sitosterol (and) Sucrose Stearate (and) Sucrose Distearate (and) Cetyl Alcohol (and) Stearyl Alcohol (Crystalcast MM, MMP), 2.00

C.
Disodium EDTA, 0.10
Xanthan Gum, 0.30
Scleroglucan (Clearogel CS 11D, MMP), 0.10
Polyglycerin-3 (Polycast 3, MMP), 2.50
Preservatives, 0.30
Paraffin (and) C18-70 Isoparaffin (and) Zinc Oxide (Sofmetic LMP-ZnO, MMP), 20.00
Dimethicone (Clearocast 100, MMP), 1.20
Isododecane (and) Isononyl Isononanoate (Clearocast 550, MMP), 5.00
Aluminum Starch Octenylsuccinate, 2.00

Procedure: Add A to main vessel and begin heating to 80-85°C. At temperature, add B to A and begin mixing with propeller agitation, holding at temperature for 30 min. Homogenize for 15 min. Add C to AB and continue mixing. Begin cooling and homogenize for 5 min at 34°C.