Soft Solid Antiperspirant

Jun 5, 2007 | Contact Author | By: Katie Schaefer
Contact the Author
Save
This item has been saved to your library.
View My Library
(click to close)
Save to My Library
Title: Soft Solid Antiperspirant
  • Article

New Phase Technologies

A.
C20-40 Alcohols (Performacol 425 Alcohol, New Phase Technologies) 4.00%w/w
Polyethylene (Performalene 400 Polyethylene, New Phase Technologies) 1.00
Cyclopentasiloxane (SF1202, General Electric) 60.00
Dimethicone (SF96-100, General Electric) 10.00
B.
Aluminum zirconium tetrachlorohydrex GLY (Reach AZP-908, Reheis) 25.00

Procedure: Heat A  to 92-95ºC. Mix until dispersed and uniform while keeping covered. Add B to A with high shear mixing. After fully dispersed, remove from heat.