Application/Category Sponsored by
Company: R.T. Vanderbilt Co., Inc.
| A. | |
| Water (aqua) | 77.00%w/w |
| B. | |
| Bentonite (Vanatural, R.T. Vanderbilt) | 2.50 |
| C. | |
| Glycerin | 5.00 |
| D. | |
| Cetearyl alcohol (and) PEG-40 castor oil (and) sodium cetearyl sulfate (Emulgade F, Cognis) | 5.00 |
| Potassium cetyl phosphate (Arlatone MAP 160K, Uniqema) | 0.50 |
| Dicaprylyl carbonate (Cetiol CC, Cognis) | 5.00 |
| C12-15 alkyl ethylhexanoate (Finester EH-25, Finetex) | 5.00 |
| E. | |
| Preservative | qs |
| Fragrance (parfum) | qs |
Procedure: While heating A to 80° C, slowly add B while mixing at maximum available shear. Mix until fully hydrated. Add C, mixing until uniform. Maintain 80° C. Separately combine D and heat to 80° C. Add D to batch with good agitation and mix until uniform. Cool with mixing. Add E when the batch reaches <30° C.