Figure 2. pH curve at 1% w/w polymer solids

The viscosity of 1% w/w polymer solids in the pH range of 5.5–11; the IE-acrylate copolymer provided excellent and consistent viscosity around 45,000 mPa•s above pH 6.5 but showed less thickening efficiency at pH 5.5-6.5.